Why are Superalloys so Special (Updated)

Why are Superalloys so Special (Updated)

Why are Superalloys so Specialnbsp (Updated)

Well, if superalloys are so important to technology, they must have some unique property! What is it?

Unfortunately, the definition of superalloys fails a bit here. For the sake of simplicity, every time I say “superalloy” in this article, you can assume I mean “nickel-based superalloy.”

Nickel-based superalloys have an amazing microstructure that gives the material excellent high-temperature properties, but there are other alloy systems that are called “superalloys” simply because they have good high-temperature properties (without the special microstructure).

Before I explain this microstructure, however, I want to show you a graph of yield strength vs temperature.

Yield strength is the most basic measurement of strength that engineers use (you can check out?this article?if you want a deeper explanation).?

As you can probably guess, as temperature increases, strength should decrease. Thermal energy means atoms vibrate faster, so they are more likely to slip past each other. In almost all materials, increasing temperature decreases strength.

Nickel-based superalloys are the exception, as you saw in the graph. As temperature increases, there is a “hump” of increased strength. This is called?anomalous yield strength?because the strength doesn’t behave normally.

The anomalous yield strength means that–at a high fraction of its melting point–nickel-based superalloys have a much higher strength than most materials. That’s why they are so good at high temperatures.?

Nickel-based superalloys have an anomalous yield strength because of their unique γ/γ’ microstructure (pronounced gamma, gamma prime).

The reason that the microstructure does this is pretty complicated, and hard to understand without a background in materials science. I’ll walk you through the full explanation in another article. I was frustrated that I never learned this in undergrad, so if you want me to use words you don’t know right now, the anomalous yield strength is because of partial dislocation cross-slip locking.

But enough about that–what is gamma and gamma prime?

Gamma is the 3rd letter in the Greek alphabet, γ. For whatever reason, this has historically been the letter that refers to an FCC phase. γ is also used to refer to austenite in steel (because austenite is FCC).

FCC means “Face-Centered Cubic.” It is one of the most common–and most stable–crystal structures. To understand what the FCC crystal looks like, imagine a cube with an atom on each corner of the cube, and each face of the cube. That’s what FCC is!

γ’ is an intermetallic compound, with L12?structure. This is an?ordered?FCC arrangement.

γ’ has Ni atoms on the faces and a different kind of atom on the corners. Usually, this other atom is Al.

Let’s look at a mixture of 75% Ni 25% Al to illustrate the difference between γ and γ’.

γ is an FCC substitutional solution. Pure Ni would be a regular FCC, as you saw previously. However, Al can dissolve in Ni. Supposing that 25% Al could dissolve in Ni, you would get something like the image on the left. ? of the Ni atoms would be randomly replaced by Al (if you aren’t sure how I counted atoms to see that ? of them are Al, I recommend you read?this article).

In γ’, the structure has an order. The Al atoms always sit on the corner, and Ni will sit on the faces. It’s possible that γ’ could have substitution as well–there is not some law preventing Ni from going to the corners, but the image on the right shows the preferred state. If there is preference for the atoms to order like this, the phase is L12. If there is no preference, the phase is just FCC.

It’s difficult to explain much about γ’ without explaining dislocations, but I’ll do my best. The combination of γ and γ’ is great because γ is tough and holds the hard?γ’ together. The alloy benefits from strength?and?toughness because of the precipitate/matrix relationship.

This kind of strengthening is called?precipitate strengthening?and is common in most advanced alloys.

?γ’ is additionally special because it is?coherent.

It turns out that the distance between atoms in Ni and Ni3Al is not very large. Ni3Al might be 1% smaller than the rest of the γ lattice. As a result, the interface between γ’ and γ is connected. This is not true in incoherent precipitates (more common).

If you imagine that a row of atoms needs to slide past another row, the connected interface between γ and γ’ allows this to be possible. This is what makes γ’ precipitates tougher than most other kinds of precipitates. There is lattice strain so sliding the atoms past each other is not easy, but it is possible.

With incoherent precipitates, the difference between the matrix and precipitate is abrupt. There is no way to push a row of atoms in the matrix, because they wouldn’t connect to the precipitate. If enough force tried to push a row of atoms past each other, the material may just develop a crack.

In addition to precipitate strengthening, superalloys benefit from?solid solution strengthening. This kind of strengthening is present in all alloys, but it is especially noteworthy in superalloys because these alloys are so well-developed that a commercial superalloy may have a dozen elements in it.

Find out more about the heat-resistant properties of our superalloys and their various applications on our website, or?contact a member of our Sales team?to talk about your requirements.

For more details on the heat-resistant properties of these superalloys and their applications, visit our website or contact our Sales team.

Explore further at www.pmisteel.com or reach out to us at [email protected].

PMI INDUSTRY is a professional supplier in China specializing in the production of nickel-based alloy bars.

要查看或添加评论,请登录

Ray Ping的更多文章

社区洞察

其他会员也浏览了